Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 7000 cP | 7000 cP | RVT Spindle 3 @ 20 rpm |
Palm Labs Adhesives TURBO-LOCK SERIES 15 Anaerobic Thread Locking Compound TURBO-LOCK 15 SERIES is a fast curing, large bolt, RED, high strength, anaerobic thread-locking compound for bonding and sealing threads. Prevents rusting of threads. It is highly resistance to heat.. |
|||
Brookfield Viscosity | 7000 cP | 7000 cP | 20 rpm aged 2 hrs, See note 1; SPI-VD-T1 |
Formosa Plastics Formolon® 24A PVC PVC Homopolymer Dispersion Resin F-24A is a low molecular weight PVC homopolymer dispersion resin which has been developed primarily for use in chemically expanded compounds as well as other applica.. |
|||
Brookfield Viscosity | 7000 cP | 7000 cP | 2 rpm aged 2 hrs, See note 1; SPI-VD-T1 |
Formosa Plastics Formolon® 28 PVC PVC Homopolymer Dispersion Resin F-28 is a high molecular weight PVC homopolymer dispersion resin which exhibits low paste viscosities as well as low residual surfactant content. This product was de.. |
|||
Brookfield Viscosity | 7000 cP @Temperature 25.0 °C |
7000 cP @Temperature 77.0 °F |
|
Loctite® 3701 Acrylic Light Cure Adhesive Acrylic Light Cure AdhesivesVersatile Loctite® ultraviolet (UV) and visible light curing adhesives can be used in bonding, encapsulating, coating, tacking, and sealing applications. These single co.. |
|||
Brookfield Viscosity | 7000 - 22500 cP | 7000 - 22500 cP | RVF #6 sp. @ 20 rpm |
3M Scotch-Seal™ 2084 Metal Sealant Features: 3M™ Scotch-Seal™ Metal Sealant 2084 is a one-part aluminum colored sealant which air dries to a tough, flexible film that resists water, oils and fuel. Retains sealing properties after e.. |
|||
Brookfield Viscosity | 7000 cP @Temperature 191 °C |
7000 cP @Temperature 375 °F |
|
3M Scotch-Weld™ 3779 Hot Melt Adhesive High heat resistance; High strength; Good fuel and oil resistance and ElectronicsInformation provided by 3M |
|||
Brookfield Viscosity | 7000 - 13000 cP | 7000 - 13000 cP | Accelerator, RVF #7 spindle, 20 rpm @ 27°C |
3M Scotch-Weld™ DP100 Plus Clear Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP100 Plus Clear is a fast setting, two-part, 1:1 mix ratio mercaptan-cured epoxy adhesive. It is a unique among fast setting mercaptan cure epoxies in that it comb.. |
|||
Brookfield Viscosity | 7000 - 20000 cP | 7000 - 20000 cP | RVT 'T-spindle' C |
3M Scotch-Weld™ ECI Gel General Purpose Instant Adhesive 3M™ Scotch-Weld™ General Purpose Instant Adhesives are single component, high strength ethyl cyanoacrylate adhesive designed to bond to a variety of substances including most plastics, rubbers, me.. |
|||
Brookfield Viscosity | 7000 cP | 7000 cP | Thermosel using spindle #27 |
3M Scotch-Weld™ EZ250015 Polyurethane Reactive (PUR) Easy 250 Wood Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive (PUR) Easy 250 Wood Adhesive is 100% solid, warm temperature applied, moisture curing urethanes. This product bonds well to wood and wood bases surfaces as w.. |
|||
Brookfield Viscosity | 7000 cP | 7000 cP | Thermosel using spindle #27 |
3M Scotch-Weld™ EZ250060 Polyurethane Reactive (PUR) Easy 250 Wood Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive (PUR) Easy 250 Wood Adhesive is 100% solid, warm temperature applied, moisture curing urethanes. This product bonds well to wood and wood bases surfaces as w.. |
|||
Brookfield Viscosity | 7000 cP | 7000 cP | Accelerator, RVF #7 sp. @20 rpm at 27°C |
3M Scotch-Weld™ LSB90 Flexible Epoxy 3M™ Scotch-Weld™ Epoxy Adhesive LSB90 is a high performance, two-part, flexible epoxy adhesive offering high shear and peel adhesion and very high levels of durability. It has a 90 minute worklife.. |
|||
Brookfield Viscosity | 7000 cP | 7000 cP | Thermosel using spindle #27 |
3M Scotch-Weld™ TE040 Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |
|||
Brookfield Viscosity | 7000 cP | 7000 cP | Thermosel using spindle #27 |
3M Scotch-Weld™ TE100 Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |
|||
Brookfield Viscosity | 7000 cP @Temperature 23.9 °C |
7000 cP @Temperature 75.0 °F |
Mixed |
BCC Products BC 7062-2H Epoxy Casting BC 7062 are aluminum filled, low viscosity epoxy mass casting resins. These room temperature cure systems allow the user choice thicknesses of 1/8 inch to a maximum of 6 inches without foaming or yi.. |
|||
Brookfield Viscosity | 7000 - 20000 cP | 7000 - 20000 cP | RVT 'T-spindle' C @ 5 |
3M Scotch-Weld™ PR Gel Plastic and Rubber Instant Adhesive 3M™ Scotch-Weld™ Plastic and Rubber Instant Adhesive is designed to give exceptional performance on difficult-to-bond plastic and rubber substrates. This adhesive may be bonded to like substrates .. |
|||
Brookfield Viscosity | 7000 - 20000 cP | 7000 - 20000 cP | RVT 'T-spindle' C @ 20 rpm |
3M Scotch-Weld™ SI Gel Surface Insensitive Instant Adhesive 3M™ Scotch-Weld™ Surface Insensitive Adhesives bond rough, porous, contaminated, and acidic substrates including wood, cardboard, veneer, fabric, cork, and leather. SI Gel (formerly SB09) is a fas.. |
|||
Brookfield Viscosity | 7000 - 15000 cP | 7000 - 15000 cP | Accelerator, RFV #7 at 20 rpm |
3M Scotch-Weld™ DP190 Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP190 Translucent is a 1:1 mix ratio similar to Scotch-Weld™ Epoxy Adhesive 2216 B/A Translucent but faster curing.Information provided by 3M |
|||
Brookfield Viscosity | 7000 cP | 7000 cP | Thermosel using spindle #27 |
3M Scotch-Weld™ TE015 Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |