Physical Properties Metric English Comments
Brookfield Viscosity 60 - 70 cP
60 - 70 cP
RVT Spindle #2, 20 RPM, 23°C, 15% T.S. in MEK
Lubrizol ESTANE® 5778 Ester Based Thermoplastic Polyurethane
Features: It is especially well suited for dispersing co-ferrite as well as Cr02 pigments used in video, audio, and data storage applications. This product offers excellent hydrolytic stability unde..