Polymer Property : Brookfield Viscosity = 64 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Brookfield Viscosity 64 cP

@Temperature 23.9 °C
64 cP

@Temperature 75.0 °F
Part A
BCC Products BC 8400 Urethane Casting
BC8400 is an unfilled, low viscosity, quick setting two component urethane system. When properly cured, BC 8400 will exhibit high impact strength and yield thermoplastic-like parts. Some features i..
Brookfield Viscosity 64 cP

@Temperature 23.9 °C
64 cP

@Temperature 75.0 °F
Part A
BCC Products BC 8405 Urethane Casting
BC8405 is an unfilled, low viscosity, quick setting two component urethane system. When properly cured, BC 8405 will exhibit high impact strength and yield thermoplastic-like parts. Some features i..