Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 5300 - 6300 cP | 5300 - 6300 cP | Zeon Test #170 |
Zeon Chemicals Nipol® DN601 Liquid Nitrile Elastomer Nipol DN 601 is a developmental liquid copolymer of butadiene and acrylonitrile containing reactive carboxyl groups. This polyme ris suggested for resin modification in adhesives and coatings.Carbox.. |