Zeon Chemicals Nipol® DN601 Liquid Nitrile Elastomer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Zeon Chemicals
Trade Name Nipol®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zeon Chemicals Nipol® DN601 Liquid Nitrile Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nipol DN 601 is a developmental liquid copolymer of butadiene and acrylonitrile containing reactive carboxyl groups. This polyme ris suggested for resin modification in adhesives and coatings.Carboxylated liquid nitrile suggested for resin modification in adhesives and coatings.
Physical Properties Metric English Comments
Specific Gravity 0.980 g/cc
0.980 g/cc
Brookfield Viscosity 5300 - 6300 cP
5300 - 6300 cP
Zeon Test #170
Ash <= 0.80 %
<= 0.80 %
Descriptive Properties Value Comments
AO Type NS
Bound ACN (%, acrylonitrile) 20
Heat Loss (%) Max 1.3
Hot/Cold C