Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 15000 - 45000 cP | 15000 - 45000 cP | DOP 60phr; ASTM D1824 |
LG Chemical PB1120 PVC General Description: PB1120, homopolymer made by micro-suspension seeded polymerization, is medium-viscosity PVC resin with pseudo plastic flow property. It can be used for foam flooring layer and w.. |
|||
Brookfield Viscosity | 35000 - 45000 cP @Temperature 25.0 °C |
35000 - 45000 cP @Temperature 77.0 °F |
RVT, Spindle #6 @ 20rpm |
Lord Adhesives Metech 3524D Silver Conductor Composition This silver conductor composition is designed for machine-dipped edge termination applications requiring nickel barrier plating. It fires to a highly dense film which is resistant to acidic plating .. |
|||
Brookfield Viscosity | 25000 - 45000 cP | 25000 - 45000 cP | RVF #6 sp. @ 20 rpm |