3M 800 Industrial Sealant

Category Polymer , Thermoset
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 800 Industrial Sealant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Scotch-Seal™ Industrial Sealant 800 is a reddish brown, brushable sealant that air dries to a flexible seal that resists water, oils and fuel and adheres to many metallic surfaces and has a useful temperature range of -65° to 200°F (-54 to 93°C).Information provided by 3M
Physical Properties Metric English Comments
Solids Content 50 - 59 %
50 - 59 %
Brookfield Viscosity 25000 - 45000 cP
25000 - 45000 cP
RVF #6 sp. @ 20 rpm
Mechanical Properties Metric English Comments
Elongation at Break 750 %
750 %
Conditioning, 4 week at 71°C
860 %
860 %
Conditioning, 7 week at 71°C
1040 %
1040 %
Conditioning, 1 week at RT/50% RH
1370 %
1370 %
Conditioning, 1 week at 71°C
Thermal Properties Metric English Comments
Flash Point -6.70 °C
19.9 °F
Processing Properties Metric English Comments
Cure Time 5.00 - 10.0 min
0.0833 - 0.167 hour
Tack Free Time
Shelf Life 15.0 Month
15.0 Month
Descriptive Properties Value Comments
Drying time 1-3 days