Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 4300 - 4700 cP | 4300 - 4700 cP | DOP 60phr, 6RPM; ASTM D1824-90 |
LG Chemical LP090 PVC General Description: LP090 ,Homopolymer made from micro-suspension polymerization ,is a medium-viscosity PVC resin with a pseudo plastic flow property in processing range. LP090 can be used for wall.. |