Polymer Property : Brookfield Viscosity = 4300 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Brookfield Viscosity 4300 - 4700 cP
4300 - 4700 cP
DOP 60phr, 6RPM; ASTM D1824-90
LG Chemical LP090 PVC
General Description: LP090 ,Homopolymer made from micro-suspension polymerization ,is a medium-viscosity PVC resin with a pseudo plastic flow property in processing range. LP090 can be used for wall..