Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 34 - 44 cP | 34 - 44 cP | |
3M Scotch-Weld™ EC40 General Purpose Instant Adhesive 3M™ Scotch-Weld™ General Purpose Instant Adhesives are single component, high strength ethyl cyanoacrylate adhesive designed to bond to a variety of substances including most plastics, rubbers, me.. |