3M™ Scotch-Weld™ General Purpose Instant Adhesives are single component, high strength ethyl cyanoacrylate adhesive designed to bond to a variety of substances including most plastics, rubbers, metals, and other common substrates. They are available in a wide variety of viscosities. General Purpose, fast curing. It is recommended for use on assemblies with close-fitting parts and smooth, even surfacesInformation provided by 3M
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
Uncured
Viscosity 34 - 44 cP
34 - 44 cP
ISO 3104/3105
Brookfield Viscosity 34 - 44 cP
34 - 44 cP
Mechanical Properties Metric English Comments
Tensile Strength at Break 20.0 MPa
2900 psi
cured; ISO 6922
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 82.0 °C
180 °F
Minimum Service Temperature, Air -54.0 °C
-65.2 °F
Processing Properties Metric English Comments
Cure Time 0.167 - 0.500 min
0.00278 - 0.00833 hour
Time to Handling Strength
1440 min
24.0 hour
Full Cure
Descriptive Properties Value Comments
Appearance Clear liquid