Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 3.6 cP | 3.6 cP | One Day, V12, Geon® 1010 |
PolyOne Geon™ 170 Series 173 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Note: Plastisol Formulation F1 consists of 100 parts of this resin + 60 parts DOP. Note: Plastisol Formulation F2 consists of 100 parts of this resin + 57 parts DOP + 3 parts ESO + 2 parts Synpron®.. |
|||
Brookfield Viscosity | 3.6 cP | 3.6 cP | One Day, V12, Geon® 1010 |
PolyOne Geon™ 170 Series 179 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Note: Plastisol Formulation F1 consists of 100 parts of this resin + 60 parts DOP. Note: Plastisol Formulation F2 consists of 100 parts of this resin + 57 parts DOP + 3 parts ESO + 2 parts Synpron®.. |