Polymer Property : Brookfield Viscosity = 3.6 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Brookfield Viscosity 3.6 cP
3.6 cP
One Day, V12, Geon® 1010
PolyOne Geon™ 170 Series 173 Polyvinyl Chloride Homopolymer (PVC Homopolymer)
Note: Plastisol Formulation F1 consists of 100 parts of this resin + 60 parts DOP. Note: Plastisol Formulation F2 consists of 100 parts of this resin + 57 parts DOP + 3 parts ESO + 2 parts Synpron®..
Brookfield Viscosity 3.6 cP
3.6 cP
One Day, V12, Geon® 1010
PolyOne Geon™ 170 Series 179 Polyvinyl Chloride Homopolymer (PVC Homopolymer)
Note: Plastisol Formulation F1 consists of 100 parts of this resin + 60 parts DOP. Note: Plastisol Formulation F2 consists of 100 parts of this resin + 57 parts DOP + 3 parts ESO + 2 parts Synpron®..