Polymer Property : Brookfield Viscosity = 26 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Brookfield Viscosity 14 - 26 cP
14 - 26 cP
25% Toluene Solution at 25°C; KM 05
Kraton® D4274B (O/E SBS) Branched Block Copolymer
Description: Kraton® D4274B is an oiled, branched copolymer based on styrene and butadiene with bound styrene in the neat polymer of 49% mass. It is supplied from South America in the physical fo..