Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 14 - 26 cP | 14 - 26 cP | 25% Toluene Solution at 25°C; KM 05 |
Kraton® D4274B (O/E SBS) Branched Block Copolymer Description: Kraton® D4274B is an oiled, branched copolymer based on styrene and butadiene with bound styrene in the neat polymer of 49% mass. It is supplied from South America in the physical fo.. |