Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 25 cP | 25 cP | 20 rpm; ASTM D1417 |
Polimeri Europa Europrene Latice® B 010 Styrene - Butadiene Copolymer Europrene Latice® B 010 is an aqueous anionic dispersion of a styrene-butadiene copolymer with medium solid content obtained by emulsion polymerization using fatty acid soap as emulsifier. It does.. |
|||
Brookfield Viscosity | 25 cP | 25 cP | (spindle=1, 20 rpm); ASTM D1417 |
Nitriflex Nitrilatex PDL 571 Carboxylated Acrylonitrile Butadiene Latex NITRILATEX synthetic lattices are divided into several groups, modified or not with carboxylic acid. Applications: NITRILATEX synthetic lattices are specially indicated to impregnate cords, adhesive.. |
|||
Brookfield Viscosity | 25 - 400 cP | 25 - 400 cP | #2/20 rpm |
Mallard Creek Polymers ROVENE® 4041 SBR Latex ROVENE® 4041 is a freeze-thaw stable carboxylated styrene-butadiene emulsion that can be used as a modifier for concrete applications. Concrete modified with ROVENE® 4041 is much tougher, more.. |
|||
Brookfield Viscosity | 25 - 50 cP | 25 - 50 cP | Spindle # 2, rpm 60 |
Michelman® FiberMax® 105B Strength enhancing fiber treatment Description: Strength enhancing fiber treatmentUsage: FibreMax® 105B is a new alternative to paraffin wax for treating medium. It is a repulpable, machine ready, fiber treatment that increases th.. |
|||
Brookfield Viscosity | 25 - 5000 cP | 25 - 5000 cP | Spindle # 4, rpm 60 |
Michelman® Hydrosize® U10-01 Polyurethane Solution Description: Polyurethane SolutionUsage: Hydrosize® U10-01 is a sizing for fiber reinforcements and is ideal for continuous strand and long fiber reinforced composites.Application data: Water Sol.. |
|||
Brookfield Viscosity | 25 - 5000 cP | 25 - 5000 cP | Spindle # 4, rpm 60 |
Michelman® Hydrosize® U6-01 Polyurethane solution Description: Polyurethane solutionUsage: Hydrosize® U6-01 is an aqueous polyurethane solution designed to be used as a fiber sizing agent for continuous nylon and epoxy reinforcements.Information.. |
|||
Brookfield Viscosity | <= 25 cP | <= 25 cP | Spindle # 3, rpm 60 |
Michelman® Michem® In-Line Primer Q4324A Primer Description: Michem® In-Line Primer Q4324A is for use with HP Indigo press W7200.Usage: Michem® In-Line Primer Q4324A is designed as a primer for HP Indigo substrates to render them compatible.. |
|||
Brookfield Viscosity | <= 25 cP | <= 25 cP | Spindle # 1, rpm 60 |
Michelman® Michem® Lube 180 Anionic co-emulsion of carnauba and paraffin waxes Description: Anionic co-emulsion of carnauba and paraffin waxesUsage: Michem® Lube 180 can provide slip, release and anti-blocking properties in a number of applications from wood coatings to bei.. |
|||
Brookfield Viscosity | <= 25 cP | <= 25 cP | Spindle # 1, rpm 60 |
Michelman® Mold Release 225SS Synthetic wax emulsion Description: Solvent based, synthetic wax emulsionUsage: Mold Release 225SS is a solvent based mold release agent suitable for use with ceramics.Information provided by Michelman® |
|||
Brookfield Viscosity | <= 25 cP | <= 25 cP | Spindle # 3, rpm 60 |
Michelman® Michem® In-Line Primer Q4304A Primer Description: Michem® In-Line Primer Q4304A is primer for print receptivity for use with HP Indigo press W3250.Usage: Michem® In-Line Primer Q4304A is designed as a primer for HP Indigo substra.. |