Polimeri Europa Europrene Latice® B 010 Styrene - Butadiene Copolymer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Styrene Butadiene Rubber
Manufacturer Polimeri Europa (Former EniChem)
Trade Name Europrene Latice®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Europrene Latice® B 010 Styrene - Butadiene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Europrene Latice® B 010 is an aqueous anionic dispersion of a styrene-butadiene copolymer with medium solid content obtained by emulsion polymerization using fatty acid soap as emulsifier. It does not contain any antioxidant.Key Features: Europrene Latice® B 010 is mainly blended with other styrene-butadiene lattices or natural latex to increase stiffness.Main Applications: Europrene Latice® 5570 is used as a reinforcing latex.Information provided by Polimeri Europa.
Physical Properties Metric English Comments
Solids Content 52 %
52 %
Total; ASTM D1417
pH 11.5
11.5
ASTM D1417
Brookfield Viscosity 25 cP
25 cP
20 rpm; ASTM D1417
Chemical Properties Metric English Comments
Styrene Content 82 %
82 %
Bound; ASTM D5775