Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 30 - 238 cP | 30 - 238 cP | RP-1107 |
Solvay RHODOLINE® 111 Surfactant Description: Hydrophobic copolymer dispersant. Highly versatile, flat to gloss, interior/exterior, low foam, excellent water resistanceIdentification: AQUEOUS SOLUTION OF POLY CARBOXYLIC ACID SALT A.. |