Polymer Property : Brookfield Viscosity = 30 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Brookfield Viscosity 30 cP
30 cP
20 rpm; ASTM D1417
Polimeri Europa Europrene Latice® 2620 Acrylonitrile-Butadiene Copolymer
Europrene Latice® 2620 is an aqueous anionic dispersion of an acrylonitrile-butadiene copolymer with low solid content obtained by emulsion using rosin acid soap as emulsifier. It contains a non s..
Brookfield Viscosity 30 - 120 cP
30 - 120 cP
#2/20 rpm
Mallard Creek Polymers ROVENE® 6050 Acrylic Emulsion
ROVENE® 6050 is a very soft acrylic latex emulsion specifically designed for formulation of permanent label adhesives. Its relative high molecular weight allows the formulation of permanent label..
Brookfield Viscosity 30 - 100 cP
30 - 100 cP
Spindle # 2, rpm 60
Michelman® Michem® Emulsion 52830 Anionic polyethylene wax emulsion
Description: Anionic polyethylene wax emulsionUsage: Michem® Emulsion 52830 as an additive provides water resistance for stucco coatings as well as release for anti-graffiti coatings.We serve man..
Brookfield Viscosity 30 - 110 cP

@Temperature 25.0 °C
30 - 110 cP

@Temperature 77.0 °F
LVT, Spindle #1 @ 60rpm
Lord Adhesives Flocklok® 851 Flock Adhesive
Flocklok® 851 is a moisture curing, polyurethane flock adhesive used to adhere flock to SBR, thermoplastic elastomers, and plastic (i.e., ABS). Thermoplastic elastomers will require the use of a ..
Brookfield Viscosity <= 30 cP
<= 30 cP
Spindle # 1, rpm 60
Michelman® RustBan® 105 Corrosion inhibitor coating
Description: Corrosion inhibitor coatingUsage: RustBan® 105 is a Vapor Corrosion Inhibitor for corrugated, solid fiber and other forms of paper board packaging to protect ferrous metals. This pro..
Brookfield Viscosity 30 - 35 cP
30 - 35 cP
Spindle # 3, rpm 60
Michelman® Sapphire 5.0 Ink Primer
Primer for use with HP Indigo press.Q4310A (Sapphire 5.0) is designed as a primer for HP Indigo substrates to render them compatible to ink. It can be used on paper substrates.Q4310A (Sapphire 5.0) ..
Brookfield Viscosity <= 30 cP
<= 30 cP
Spindle # 1, rpm 60
Michelman® Michem® Coat 218Cl4AF Corrosion inhibitor coating
Description: Corrosion inhibitor coatingUsage: Michem® Coat 218CI4AF is a contact type corrosion inhibitor. This coating is used to protect electrical components, metal parts, and sensitive paper..
Brookfield Viscosity 30 cP

@Temperature 25.0 °C
30 cP

@Temperature 77.0 °F
Loctite® FLASHCURE™ 4302 Light Cure Instant Adhesive
Cyanoacrylate Light Cure AdhesivesLoctite offers the most comprehensive line of adhesives and sealants available to the medical device industry. These USP class VI and/or ISO-10993 compliant product..
Brookfield Viscosity 30 - 238 cP
30 - 238 cP
RP-1107
Solvay RHODOLINE® 111 Surfactant
Description: Hydrophobic copolymer dispersant. Highly versatile, flat to gloss, interior/exterior, low foam, excellent water resistanceIdentification: AQUEOUS SOLUTION OF POLY CARBOXYLIC ACID SALT A..
Brookfield Viscosity 30 cP
30 cP
DuPont Performance Polymers AquaStik® AQS-2540 Polychloroprene Latex  (discontinued **)
Aquastik™ polychloroprene latexes have been designed for the adhesives industry. They provide an environmentally friendly alternative to solvent-borne systems.This grade features post-forming. 59..