Polymer Property : Brookfield Viscosity = 22000 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Brookfield Viscosity 22000 cP

@Temperature -15.0 °C
22000 cP

@Temperature 5.00 °F
ASTM D2983
ExxonMobil Synesstic™ 12 Synthetic Fluid
Product Description: Synesstic™ Alkylated Naphthalene (AN) represent a unique class of API Group V category fluids. Synesstic™ AN products offer improved hydrolytic, thermal and oxidative stabilit..
Brookfield Viscosity 22000 cP
22000 cP
Base, RVF #7 sp. @20 rpm at 27°C
3M Scotch-Weld™ LSB90 Flexible Epoxy
3M™ Scotch-Weld™ Epoxy Adhesive LSB90 is a high performance, two-part, flexible epoxy adhesive offering high shear and peel adhesion and very high levels of durability. It has a 90 minute worklife..
Brookfield Viscosity 22000 - 33000 cP
22000 - 33000 cP
Accelerator, RVF #7 spindle, 20 rpm @ 27°C
3M Scotch-Weld™ DP125 Translucent Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP125 Translucent is a faster curing version of 3M Scotch-Weld Epoxy Adhesive 2216 Translucent B/A. The worklife and cure time has been reduced from hours and days ..