Polymer Property : Brookfield Viscosity = 21000 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Brookfield Viscosity 21000 cP
21000 cP
2 rpm aged 2 hrs, See note 1; SPI-VD-T1
Formosa Plastics Formolon® 34 PVC
PVC Homopolymer Dispersion Resin F-34 is a medium molecular weight PVC homopolymer dispersion resin which has been developed primarily for use in chemically expanded compound. In expanded systems, t..