Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 2.95 cP @Temperature -40.0 °C |
2.95 cP @Temperature -40.0 °F |
One Day, V2, ALTC-22 |
PolyOne Geon™ 210 Series 218 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Note: Plastisol and or Fused Film Formulation F2 consists of 60 parts of Geon®178 + 40 parts of this resin + 57 parts DOP + 3 parts ESO + 2 parts Synpron® 940 Note: Plastisol Formulation F1 consis.. |