Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Geon™ 210 Series 218 Polyvinyl Chloride Homopolymer (PVC Homopolymer)

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ 210 Series 218 Polyvinyl Chloride Homopolymer (PVC Homopolymer).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Note: Plastisol and or Fused Film Formulation F2 consists of 60 parts of Geon®178 + 40 parts of this resin + 57 parts DOP + 3 parts ESO + 2 parts Synpron® 940 Note: Plastisol Formulation F1 consists of 60 parts of 178 + 40 parts of this resin + 60 parts DOP Note: The values set forth represent typical values and PolyOne Corporation, therefore, makes no representation that the material in any particular shipment will conform to the listed properties. Packaging: This resin is shipped in multi-wall paper bags, net weight 50 lbs, 2500 lbs per pallet. Information shown on the package includes commercial identification number, lot and weight. Shipping: This resin can be shipped in 45,000 lb bulk trucks and 180,000 lb bulk railcars.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.40 g/cc
1.40 g/cc
ASTM D792
Density 0.561 g/cc
0.0203 lb/in³
ASTM D1505
Loss On Ignition 0.10 %
0.10 %
Bagged, Geon® 793
Particle Size 70 µm
70 µm
Geon® 812
Particle Mesh Size 120 Mesh
120 Mesh
4%; Geon® 812
Relative Viscosity 1.93 cP
1.93 cP
1% Cyclohexanone
Brookfield Viscosity 3.4 cP
3.4 cP
Initial, V12, Geon® 1010
4.0 cP
4.0 cP
One Day, V12, Geon® 1010
2.95 cP

@Temperature -40.0 °C
2.95 cP

@Temperature -40.0 °F
One Day, V2, ALTC-22
3.0 cP

@Temperature -40.0 °C
3.0 cP

@Temperature -40.0 °F
One Day, V20
Viscosity Measurement 0.74
0.74
Inherent; ASTM D1243-60-A
Melt Flow 540 g/10 min

@Pressure 0.655 MPa
540 g/10 min

@Pressure 95.0 psi
Severs Efflux
Optical Properties Metric English Comments
Gloss 35 %

@Temperature 177 °C
35 %

@Temperature 351 °F
60°, fused 5 min, ALTC-65
63 %

@Temperature 199 °C
63 %

@Temperature 390 °F
60°, fused 3 min, ALTC-65
Descriptive Properties Value Comments
Air Release 1 min
ALTC-25
Degree of Polymerization 740
Correlation
Features Low Molecular Weight
Forms Powder
Gel Temperature 77 °C
PP
Generic Material PVC Homopolymer
Generic Name Polyvinyl Chloride Homopolymer (PVC Homopolymer)
K-Value 59
No Standard; Correlation
Polymerization Process Suspension
Processing Method Casting
Dip Coating
Rotational Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Vinyl Dispersion Gauge 155 µm
ALTC-28
Copyright © lookpolymers.com All Rights Reserved