Polymer Property : Brookfield Viscosity = 150 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Brookfield Viscosity 120 - 150 cP
120 - 150 cP
LFV #1 spindle @ 12 rpm
3M Scotch-Weld™ RT09 Retaining Compound Anaerobic Adhesives
3M™ Scotch-Weld™ Retaining Compound Anaerobic Adhesives are one-component anaerobic adhesives designed to secure cylindrical metal assemblies such as bearings on shafts, bushing, sleeves, housings..