Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 120 - 150 cP | 120 - 150 cP | LFV #1 spindle @ 12 rpm |
3M Scotch-Weld™ RT09 Retaining Compound Anaerobic Adhesives 3M™ Scotch-Weld™ Retaining Compound Anaerobic Adhesives are one-component anaerobic adhesives designed to secure cylindrical metal assemblies such as bearings on shafts, bushing, sleeves, housings.. |