Physical Properties Metric English Comments
Brookfield Viscosity 4000 - 11000 cP
4000 - 11000 cP
Base, RVF #7 spindle, 20 rpm @ 27°C
3M Scotch-Weld™ DP100 Plus Clear Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP100 Plus Clear is a fast setting, two-part, 1:1 mix ratio mercaptan-cured epoxy adhesive. It is a unique among fast setting mercaptan cure epoxies in that it comb..