Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 4000 - 20000 cP | 4000 - 20000 cP | DOP 60phr; ASTM D1824 |
LG Chemical PA1302 PVC General Description: PA1302, vinyl chloride copolymer with vinyl acetate exhibits excellent properties. It is easy to process and gives effective flow. Main Applications: Adhesive for sheet & film, .. |
|||
Brookfield Viscosity | <= 4000 cP | <= 4000 cP | Spindle # 4, rpm 60 |
Michelman® Hydrosize® HP3-02 Nonionic phenoxy dispersion Description: Nonionic phenoxy dispersionUsage: Hydrosize® HP3-02 is designed to be used as a fiber sizing coating with a high Tg and excellent adhesion.When manufactured in USA product meets food.. |
|||
Brookfield Viscosity | 4000 cP @Temperature 25.0 °C |
4000 cP @Temperature 77.0 °F |
Spindle CP40 @ 5rpm |
Lord Adhesives Thermosetâ„¢ ME-531 Underfill Encapsulant LORD Thermosetâ„¢ ME-531 encapsulant is a high purity, semiconductor grade epoxy underfill product developed for the encapsulation of flip chip devices. It is formulated to reduce warpage and wit.. |
|||
Brookfield Viscosity | 4000 cP @Temperature 25.0 °C |
4000 cP @Temperature 77.0 °F |
Toluene solution. Neat polymer concentration, 25%w. |
Kraton® D1101 (SBS) Linear Block Copolymer (SBS) styrene-butadiene-styrene block polymer. KRATON® Polymers require no premastication or vulcanization. They can be blended with thermoplastic polymers and significantly improve the impact .. |
|||
Brookfield Viscosity | 4000 cP @Temperature 25.0 °C |
4000 cP @Temperature 77.0 °F |
|
Loctite® 3102 Acrylic Light Cure Adhesive Acrylic Light Cure AdhesivesVersatile Loctite® ultraviolet (UV) and visible light curing adhesives can be used in bonding, encapsulating, coating, tacking, and sealing applications. These single co.. |
|||
Brookfield Viscosity | 4000 cP @Temperature 25.0 °C |
4000 cP @Temperature 77.0 °F |
|
Loctite® 3175 Acrylic Light Cure Adhesive Acrylic Light Cure AdhesivesVersatile Loctite® ultraviolet (UV) and visible light curing adhesives can be used in bonding, encapsulating, coating, tacking, and sealing applications. These single co.. |
|||
Brookfield Viscosity | 4000 cP @Temperature 25.0 °C |
4000 cP @Temperature 77.0 °F |
|
Loctite® 3201 Light Cure Acrylic Adhesive Medical Grade BondersLoctite offers the most comprehensive line of adhesives and sealants available to the medical device industry. These USP class VI and/or ISO-10993 compliant products are designe.. |
|||
Brookfield Viscosity | 4000 cP @Temperature 25.0 °C |
4000 cP @Temperature 77.0 °F |
|
Loctite® 3751 Acrylic Light Cure Adhesive Acrylic Light Cure AdhesivesVersatile Loctite® ultraviolet (UV) and visible light curing adhesives can be used in bonding, encapsulating, coating, tacking, and sealing applications. These single co.. |
|||
Brookfield Viscosity | 4000 - 11000 cP | 4000 - 11000 cP | Base, RVF #7 spindle, 20 rpm @ 27°C |
3M Scotch-Weld™ DP100 Plus Clear Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP100 Plus Clear is a fast setting, two-part, 1:1 mix ratio mercaptan-cured epoxy adhesive. It is a unique among fast setting mercaptan cure epoxies in that it comb.. |
|||
Brookfield Viscosity | 4000 cP @Temperature 121 °C |
4000 cP @Temperature 250 °F |
|
3M Scotch-Weld™ 3762LM Low Melt Adhesive Excellent “hot-tack”, fast setting for corrugated, beadboard, recouperage, repacking chipboard, wood; Economical, general purpose and Use with low melt applicator onlyInformation provided by 3M |
|||
Brookfield Viscosity | 4000 - 15000 cP | 4000 - 15000 cP | RVT #4 sp @ 20 rpm |
3M Scotch-Weld™ TL72 Threadlocker Anaerobic Adhesive 3M™ Scotch-Weld™ Threadlocker Anaerobic Adhesives are one-component anaerobic adhesives that cure and seal threaded assemblies that meet a wide range of applications to prevent vibration loosening.. |
|||
Brookfield Viscosity | 4000 cP @Temperature 121 °C |
4000 cP @Temperature 250 °F |
|
3M Scotch-Weld™ 3750LM Low Melt Adhesive Excellent "hot tack", fast setting for corrugated, beadboard, repack, recoup and Economical, general purpose and Use with AE II LET applicator onlyInformation provided by 3M |