Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 30 - 110 cP @Temperature 25.0 °C |
30 - 110 cP @Temperature 77.0 °F |
LVT, Spindle #1 @ 60rpm |
Lord Adhesives Flocklok® 851 Flock Adhesive Flocklok® 851 is a moisture curing, polyurethane flock adhesive used to adhere flock to SBR, thermoplastic elastomers, and plastic (i.e., ABS). Thermoplastic elastomers will require the use of a .. |