Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | <= 1.0 cP | <= 1.0 cP | RVF #3, 10 rpm, 424 |
PolyOne Aquamix™ 142 Latex Storage Stability: In excess of 6 months when stored under proper conditions in original sealed container. Keep from freezing. Water lost by evaporation can adversely affect viscosity, dispersabilit.. |
|||
Brookfield Viscosity | 1.0 - 20 cP | 1.0 - 20 cP | Spindle # 1, rpm 60 |
Michelman® CleanGrip® 111 Alumina based, nonskid coating Description: Water based frictionizing agentUsage: CleanGrip® 111 is an alumina based, nonskid coating designed to reduce the slipperiness of shipping containers by providing excellent slide angl.. |
|||
Brookfield Viscosity | 1.0 cP @Temperature 25.0 °C |
1.0 cP @Temperature 77.0 °F |
|
Loctite® 713 Accelerator for cyanoacrylates Medical Grade BondersLoctite offers the most comprehensive line of adhesives and sealants available to the medical device industry. These USP class VI and/or ISO-10993 compliant products are designe.. |
|||
Brookfield Viscosity | 1.0 - 3.0 cP @Temperature 20.0 °C |
1.0 - 3.0 cP @Temperature 68.0 °F |
Brookfield RVT spindle 2.2 RPM |
C.O.I.M. FILCO® 354 N Unsaturated Bisphenolic Polyester Polymer for Glass Fiber Sizing Description: Unsaturated Bisphenolic Polyester Polymer for Glass Fiber SizingGeneral Information: COIM has developed a range of polyesters for the treatment of glass fiber. These polyesters come in .. |