Physical Properties Metric English Comments
Brookfield Viscosity <= 1.0 cP
<= 1.0 cP
RVF #3, 10 rpm, 424
PolyOne Aquamix™ 142 Latex
Storage Stability: In excess of 6 months when stored under proper conditions in original sealed container. Keep from freezing. Water lost by evaporation can adversely affect viscosity, dispersabilit..
Brookfield Viscosity 1.0 - 20 cP
1.0 - 20 cP
Spindle # 1, rpm 60
Michelman® CleanGrip® 111 Alumina based, nonskid coating
Description: Water based frictionizing agentUsage: CleanGrip® 111 is an alumina based, nonskid coating designed to reduce the slipperiness of shipping containers by providing excellent slide angl..
Brookfield Viscosity 1.0 cP

@Temperature 25.0 °C
1.0 cP

@Temperature 77.0 °F
Loctite® 713 Accelerator for cyanoacrylates
Medical Grade BondersLoctite offers the most comprehensive line of adhesives and sealants available to the medical device industry. These USP class VI and/or ISO-10993 compliant products are designe..
Brookfield Viscosity 1.0 - 3.0 cP

@Temperature 20.0 °C
1.0 - 3.0 cP

@Temperature 68.0 °F
Brookfield RVT spindle 2.2 RPM
C.O.I.M. FILCO® 354 N Unsaturated Bisphenolic Polyester Polymer for Glass Fiber Sizing
Description: Unsaturated Bisphenolic Polyester Polymer for Glass Fiber SizingGeneral Information: COIM has developed a range of polyesters for the treatment of glass fiber. These polyesters come in ..