Polymer Property : Environmental Stress Crack Resistance = 500 hour Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Environmental Stress Crack Resistance 1.00 - 500 hour
1.00 - 500 hour
Average value: 128 hour Grade Count:4
Overview of materials for High Density Polyethylene (HDPE), Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Impact Grade". Each property range of values reported is minimum and m..
Environmental Stress Crack Resistance 2.00 - 500 hour

@Temperature 50.0 - 50.0 °C
2.00 - 500 hour

@Temperature 122 - 122 °F
Average value: 132 hour Grade Count:14
Overview of materials for High Density Polyethylene (HDPE), Injection Molded
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Injection Molded". Each property range of values reported is minimum a..
Environmental Stress Crack Resistance 168 - 500 hour
168 - 500 hour
Average value: 263 hour Grade Count:7
Overview of materials for Low Density Polyethylene (LDPE), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Film Grade". Each property range of values reported is minimum and maxi..