Polymer Property : Environmental Stress Crack Resistance = 266 hour Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Environmental Stress Crack Resistance 266 hour
266 hour
F50, Condition A
NOVA Chemicals Novapol® HB-W558-A HDPE Extrusion Resin  (discontinued **)
Molded Plaque Properties. Features: High molecular weight, excellent impact strength, high rigidity, easy processing.Applications: large part blow molding, large oil drums.Data provided by the manu..