NOVA Chemicals Novapol® HB-W558-A HDPE Extrusion Resin  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Extruded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NOVA Chemicals Novapol® HB-W558-A HDPE Extrusion Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Molded Plaque Properties. Features: High molecular weight, excellent impact strength, high rigidity, easy processing.Applications: large part blow molding, large oil drums.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 0.958 g/cc
0.0346 lb/in³
ASTM D792
Environmental Stress Crack Resistance 266 hour
266 hour
F50, Condition A
Melt Flow 5.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 30.0 MPa
4350 psi
ASTM D638
Elongation at Break 890 %
890 %
ASTM D638
Flexural Modulus 1.48 GPa
215 ksi
ASTM D790
Izod Impact, Notched 7.50 J/cm
14.1 ft-lb/in
Notched/Unnotched not specified; ASTM D256
Thermal Properties Metric English Comments
Brittleness Temperature <= -100 °C
<= -148 °F
ASTM D696
Processing Properties Metric English Comments
Melt Temperature 180 - 220 °C
356 - 428 °F