Physical Properties | Metric | English | Comments |
---|---|---|---|
Environmental Stress Crack Resistance | 180 hour | 180 hour | Igepal 10%, F50; ASTM D1693-A |
Borealis BorPURE™ MB6562 High Density Polyethylene for Injection Molding BorPure™ MB6562 is a bimodal, high-density polyethylene intended for injection and compression molding. This grade combines excellent organoleptic properties, environmental stress crack resistance .. |
|||
Environmental Stress Crack Resistance | 180 hour | 180 hour | Igepal 10%, F50; ASTM D1693-A |
Borealis BorPURE™ MB6561 High Density Polyethylene for Injection Molding BorPure™ MB6561 is a bimodal, high-density polyethylene intended for injection and compression molding. This grade combines excellent organoleptic properties, environmental stress crack resistance .. |
|||
Environmental Stress Crack Resistance | 180 hour | 180 hour | Condition B, 10%; ASTM D1693 |
ExxonMobil LL 6202.19 Injection Molding Resin Product Description: LL 6202 is a narrow molecular weight butane copolymer designed for applications that require excellent toughness. This resin offers easy processability for applications that req.. |