Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission Rate | 745 cc/m²/day @Temperature 23.0 °C |
48.0 cc/100 in²/day @Temperature 73.4 °F |
0% RH; ExxonMobil Method |
ExxonMobil Bicor™ 30MB666 OPP Film Product Description: A biaxially oriented transparent polypropylene film, acrylic coated two sides. It provides outstanding performance on all packaging machines.Availability: Africa & Middle East, .. |
|||
Oxygen Transmission Rate | 745 cc/m²/day @Temperature 23.0 °C |
48.0 cc/100 in²/day @Temperature 73.4 °F |
0% RH; ExxonMobil Method |
ExxonMobil Bicor™ 30MB668 OPP Film Product Description: A high speed transparent, biaxially oriented polypropylene film, coated one side very low temperature seal (VLTS) coating. VLTS coating provides excellent performances on high s.. |
|||
Oxygen Transmission Rate | 745 cc/m²/day @Temperature 23.0 °C |
48.0 cc/100 in²/day @Temperature 73.4 °F |
0% RH; ExxonMobil Method |
ExxonMobil Bicor™ 30MBR666 OPP Film Product Description: Bicor 30MBR is a biaxially oriented transparent polypropylene film coated with humidity resistant acrylic on both sides. This film is designed to wrap products with a high moist.. |
|||
Oxygen Transmission Rate | 745 cc/m²/day @Temperature 23.0 °C |
48.0 cc/100 in²/day @Temperature 73.4 °F |
0% RH; ExxonMobil Method |
ExxonMobil Bicor™ 32MB600 OPP Film Product Description: A biaxially oriented transparent polypropylene film, acrylic coated two sides. Gives outstanding performance on overwrap and HFFS machines.Availability: Africa & Middle East, As.. |
|||
Oxygen Transmission Rate | 745 cc/m²/day @Temperature 23.0 °C |
48.0 cc/100 in²/day @Temperature 73.4 °F |
0% RH; ExxonMobil Method |
ExxonMobil Oppalyte™ 42MH647 OPP Film Product Description: A super white opaque, modified higher density, biaxially oriented polypropylene film, acrylic coated two sides. It provides outstanding performance on all packaging machines.Ava.. |
|||
Oxygen Transmission Rate | 745 cc/m²/day @Temperature 23.0 °C |
48.0 cc/100 in²/day @Temperature 73.4 °F |
0% RH; ExxonMobil Method |
ExxonMobil Oppalyte™ 42MH648 OPP Film Product Description: A high speed super white opaque, modified higher density, biaxially oriented polypropylene film, acrylic coated one side acrylic, one side very low temperature seal (VLTS) coati.. |