Physical Properties Metric English Comments
Oxygen Transmission 208 cc-mm/m²-24hr-atm
528 cc-mil/100 in²-24hr-atm
or 12400 cc/m²-24hr-atm for the 50 gauge film. ASTM D3985
DuPont™ Clysar® VEZ Polyolefin Shrink Packaging Film, 50 Gauge  (discontinued **)
Data provided by DuPont Packaging Polymers.DuPont Clysar® VEZ is a clear, biaxially oriented, heat-shrinkable, multilayer film with one of the lowest shrink force available in the Clysar® line. C..