Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont™ Clysar® VEZ Polyolefin Shrink Packaging Film, 50 Gauge  (discontinued **)

Category Polymer , Film , Thermoplastic , Polyolefin , Polyolefin, Film Grade , Polyolefin, Film Grade (Polyolefin)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont™ Clysar® VEZ Polyolefin Shrink Packaging Film, 50 Gauge  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by DuPont Packaging Polymers.DuPont Clysar® VEZ is a clear, biaxially oriented, heat-shrinkable, multilayer film with one of the lowest shrink force available in the Clysar® line. Clysar® VEZS is a hot slip version of VEZ. DuPont Clysar® VEZ is designed for packaging items that need a low shrink force such as thin stacks of paper or boxes that tend to crush. It can also be used for packaging lightweight, low abuse products. It combines excellent optics, high-speed machinability and clean shrink appearance with the economics of high yield, reduced changeover and downtime and greater use of storage space.
Physical Properties Metric English Comments
Moisture Vapor Transmission 0.490 cc-mm/m²-24hr-atm
1.24 cc-mil/100 in²-24hr-atm
ASTM 1249
Oxygen Transmission 208 cc-mm/m²-24hr-atm
528 cc-mil/100 in²-24hr-atm
or 12400 cc/m²-24hr-atm for the 50 gauge film. ASTM D3985
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 90 %
90 %
Average; ASTM D882
Secant Modulus 0.530 GPa
76.9 ksi
Stiffness Modulus; ASTM D882
Impact Test 0.565 J
0.417 ft-lb
Spencer Impact ASTM D3420
Coefficient of Friction, Dynamic 0.21
0.21
ASTM D1894
Elmendorf Tear Strength MD 11 g
11 g
Orientation not specified; ASTM D1922
Film Tensile Strength at Break, MD 69.0 MPa
10000 psi
ASTM D882
Optical Properties Metric English Comments
Haze 2.0 %
2.0 %
ASTM D1003
Gloss 145 %
145 %
at 20°; ASTM D2457