Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Oxygen Transmission = 5.79 cc-mil/100 in²-24hr-atm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Oxygen Transmission 2.28 cc-mm/m²-24hr-atm
5.79 cc-mil/100 in²-24hr-atm
Inchem Phenoxy PKFE
Phenoxy PKFE - polyhydroxy ether of Bisphenol A. Originally developed by Union Carbide. Produced by InChem Corporation.
Copyright © lookpolymers.com All Rights Reserved