Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission | 179 cc-mm/m²-24hr-atm | 455 cc-mil/100 in²-24hr-atm | or 9400 cc/m²-24hr-atm for the film. ASTM D3985 |
DuPont™ Clysar® ABL Polyolefin Shrink Packaging Film, 75 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat shrinkable, linear low/ultra low density polyolefin film. Used where lower processing temperatures, superior pack.. |
|||
Oxygen Transmission | 179 cc-mm/m²-24hr-atm | 455 cc-mil/100 in²-24hr-atm | or 4700 cc/m²-24hr-atm for the film. ASTM D3985 |
DuPont™ Clysar® HP Polyolefin Shrink Packaging Film, 150 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat-shrinkable, linear low-density polyolefin film. Cross-linking produces a film that is extremely rugged and durab.. |
|||
Oxygen Transmission | 179 cc-mm/m²-24hr-atm | 455 cc-mil/100 in²-24hr-atm | or 4700 cc/m²-24hr-atm for the film. ASTM D3985 |
DuPont™ Clysar® LLP Polyolefin Shrink Packaging Film, 150 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, nonirradiated, heat-shrinkable, linear low-density polyolefin film. LLPS is the silicon treated, hot slip version of .. |