Polymer Property : Oxygen Transmission = 179 cc-mm/m²-24hr-atm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Oxygen Transmission 179 cc-mm/m²-24hr-atm
455 cc-mil/100 in²-24hr-atm
or 9400 cc/m²-24hr-atm for the film. ASTM D3985
DuPont™ Clysar® ABL Polyolefin Shrink Packaging Film, 75 Gauge  (discontinued **)
Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat shrinkable, linear low/ultra low density polyolefin film. Used where lower processing temperatures, superior pack..
Oxygen Transmission 179 cc-mm/m²-24hr-atm
455 cc-mil/100 in²-24hr-atm
or 4700 cc/m²-24hr-atm for the film. ASTM D3985
DuPont™ Clysar® HP Polyolefin Shrink Packaging Film, 150 Gauge  (discontinued **)
Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat-shrinkable, linear low-density polyolefin film. Cross-linking produces a film that is extremely rugged and durab..
Oxygen Transmission 179 cc-mm/m²-24hr-atm
455 cc-mil/100 in²-24hr-atm
or 4700 cc/m²-24hr-atm for the film. ASTM D3985
DuPont™ Clysar® LLP Polyolefin Shrink Packaging Film, 150 Gauge  (discontinued **)
Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, nonirradiated, heat-shrinkable, linear low-density polyolefin film. LLPS is the silicon treated, hot slip version of ..