Physical Properties Metric English Comments
Oxygen Transmission 158 cc-mm/m²-24hr-atm
401 cc-mil/100 in²-24hr-atm
or 6300 cc/m²-24hr-atm for the film. ASTM D3985
DuPont™ Clysar® HP Polyolefin Shrink Packaging Film, 100 Gauge  (discontinued **)
Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat-shrinkable, linear low-density polyolefin film. Cross-linking produces a film that is extremely rugged and durab..
Oxygen Transmission 158 cc-mm/m²-24hr-atm
401 cc-mil/100 in²-24hr-atm
or 6300 cc/m²-24hr-atm for the film. ASTM D3985
DuPont™ Clysar® LLP Polyolefin Shrink Packaging Film, 100 Gauge  (discontinued **)
Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, nonirradiated, heat-shrinkable, linear low-density polyolefin film. LLPS is the silicon treated, hot slip version of ..
Oxygen Transmission 158 - 229 cc-mm/m²-24hr-atm
401 - 582 cc-mil/100 in²-24hr-atm
Average value: 199 cc-mm/m²-24hr-atm Grade Count:8
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Film Grade". Each property range of values reported is minimum a..
Oxygen Transmission 158 cc-mm/m²-24hr-atm

@Thickness 0.0254 mm
401 cc-mil/100 in²-24hr-atm

@Thickness 0.00100 in
Based on 1 mil (0.0254 mm) thick film; ASTM D3985
DuPont Elvax® 3130 Ethylene-Vinyl Acetate Copolymer Resin for Blown Film
12 wt% Vinyl Acetate.General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent dra..
Copyright © lookpolymers.com All Rights Reserved