Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission | 158 cc-mm/m²-24hr-atm | 401 cc-mil/100 in²-24hr-atm | or 6300 cc/m²-24hr-atm for the film. ASTM D3985 |
DuPont™ Clysar® HP Polyolefin Shrink Packaging Film, 100 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat-shrinkable, linear low-density polyolefin film. Cross-linking produces a film that is extremely rugged and durab.. |
|||
Oxygen Transmission | 158 cc-mm/m²-24hr-atm | 401 cc-mil/100 in²-24hr-atm | or 6300 cc/m²-24hr-atm for the film. ASTM D3985 |
DuPont™ Clysar® LLP Polyolefin Shrink Packaging Film, 100 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, nonirradiated, heat-shrinkable, linear low-density polyolefin film. LLPS is the silicon treated, hot slip version of .. |
|||
Oxygen Transmission | 158 - 229 cc-mm/m²-24hr-atm | 401 - 582 cc-mil/100 in²-24hr-atm | Average value: 199 cc-mm/m²-24hr-atm Grade Count:8 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Film Grade". Each property range of values reported is minimum a.. |
|||
Oxygen Transmission | 158 cc-mm/m²-24hr-atm @Thickness 0.0254 mm |
401 cc-mil/100 in²-24hr-atm @Thickness 0.00100 in |
Based on 1 mil (0.0254 mm) thick film; ASTM D3985 |
DuPont Elvax® 3130 Ethylene-Vinyl Acetate Copolymer Resin for Blown Film 12 wt% Vinyl Acetate.General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent dra.. |