Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission | 1.00 - 1.95 cc-mm/m²-24hr-atm | 2.54 - 4.95 cc-mil/100 in²-24hr-atm | Average value: 1.50 cc-mm/m²-24hr-atm Grade Count:16 |
Overview of materials for Nylon 6, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Extruded". Each property range of values reported is minimum and maximum values of appropriate .. |