Physical Properties Metric English Comments
Oxygen Transmission 1.40 cc-mm/m²-24hr-atm
3.56 cc-mil/100 in²-24hr-atm
or 54 cc/m²-24hr-atm for the film at 23°C, 0% RH. ASTM D1434-66
DuPont™ Dartek® F-101 Nylon 6,6 Forming Film, 25 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.A cast nylon film made from type 6,6 polymer - the condensation product of adipic acid and hexamethylen diamine. It contains all the excellent properties ..
Oxygen Transmission 1.40 cc-mm/m²-24hr-atm
3.56 cc-mil/100 in²-24hr-atm
or 54 cc/m²-24hr-atm for the film at 23°C, 0% RH. ASTM D1434-66
DuPont™ Dartek® N-201 Nylon 6,6 Non-Forming Film, 25 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.A nylon film made from type 6,6 polymer - the condensation product of adipic acid and hexamethylene diamine. Primarily formulated for pouch and primal bag ..