Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission | 27.6 - 27.6 cc-mm/m²-24hr-atm @Temperature 40.0 - 40.0 °C |
70.1 - 70.1 cc-mil/100 in²-24hr-atm @Temperature 104 - 104 °F |
Average value: 27.6 cc-mm/m²-24hr-atm Grade Count:1 |
Overview of materials for Polychlorotrifluoroethylene; Molded This property data is a summary of similar materials in the MatWeb database for the category "Polychlorotrifluoroethylene; Molded". Each property range of values reported is minimum and maximum valu.. |