Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission | 95.0 cc-mm/m²-24hr-atm | 241 cc-mil/100 in²-24hr-atm | Average value: 95.0 cc-mm/m²-24hr-atm Grade Count:3 |
Overview of materials for Polypropylene, Sheet/Thermoforming Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Sheet/Thermoforming Grade". Each property range of values reported is minimum and maximum.. |
|||
Oxygen Transmission | 95.0 cc-mm/m²-24hr-atm | 241 cc-mil/100 in²-24hr-atm | Average value: 95.0 cc-mm/m²-24hr-atm Grade Count:10 |
Overview of materials for Polypropylene, Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Blow Molding Grade". Each property range of values reported is minimum and maximum values.. |