Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission | 5.10 - 23.0 cc-mm/m²-24hr-atm | 13.0 - 58.4 cc-mil/100 in²-24hr-atm | Average value: 11.1 cc-mm/m²-24hr-atm Grade Count:3 |
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Unreinforced". Each property range of values reported is minimum and m.. |