Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Oxygen Transmission = 11.0 cc-mm/m²-24hr-atm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Oxygen Transmission 11.0 cc-mm/m²-24hr-atm
27.9 cc-mil/100 in²-24hr-atm
ASTM D3985
Eastman Eastar 5445 PCTG Copolyester, Film  (discontinued **)
Eastar PCTG 5445 is an amorphous copolyester. Because of its clarity, toughness and good melt strength, Eastar PCTG Copolyester 5445 is useful in a number of applications. It has high gloss and is t..
Copyright © lookpolymers.com All Rights Reserved