Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 90 g/10 min @Load 5.00 kg, Temperature 266 °C |
90 g/10 min @Load 11.0 lb, Temperature 511 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® 4012G PBT (Europe-Africa-Middle East) VALOX 4012G is a 10% glass fibre reinforced PBT injection moulding resin with excellent mechanical properties. Applications: connectors. This grade is a 4012 with improved cycle time and ductility. |
|||
Melt Flow | 90 g/10 min @Load 5.00 kg, Temperature 265 °C |
90 g/10 min @Load 11.0 lb, Temperature 509 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® 4521 PBT (Europe-Africa-Middle East) VALOX 4521 is a high flow, 19.5% glass reinforced flame retardant PBT injection moulding resin. Applications: electrical applications. |
|||
Melt Flow | 90 g/10 min @Load 5.00 kg, Temperature 265 °C |
90 g/10 min @Load 11.0 lb, Temperature 509 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® 4631 PBT (Europe-Africa-Middle East) VALOX 4631 is a 30% glass reinforced, flame retarded PBT injection moulding resin with good electrical properties and excellent mechanical properties. |
|||
Melt Flow | 90 g/10 min @Load 5.00 kg, Temperature 266 °C |
90 g/10 min @Load 11.0 lb, Temperature 511 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® 4631 PBT (Europe-Africa-Middle East) VALOX 4631 is a 30% glass reinforced, flame retarded PBT injection moulding resin with good electrical properties and excellent mechanical properties. |