Physical Properties Metric English Comments
Melt Flow 90 g/10 min

@Load 5.00 kg,
Temperature 266 °C
90 g/10 min

@Load 11.0 lb,
Temperature 511 °F
ASTM D1238
SABIC Innovative Plastics Valox® 4012G PBT (Europe-Africa-Middle East)
VALOX 4012G is a 10% glass fibre reinforced PBT injection moulding resin with excellent mechanical properties. Applications: connectors. This grade is a 4012 with improved cycle time and ductility.
Melt Flow 90 g/10 min

@Load 5.00 kg,
Temperature 265 °C
90 g/10 min

@Load 11.0 lb,
Temperature 509 °F
ASTM D1238
SABIC Innovative Plastics Valox® 4521 PBT (Europe-Africa-Middle East)
VALOX 4521 is a high flow, 19.5% glass reinforced flame retardant PBT injection moulding resin. Applications: electrical applications.
Melt Flow 90 g/10 min

@Load 5.00 kg,
Temperature 265 °C
90 g/10 min

@Load 11.0 lb,
Temperature 509 °F
ASTM D1238
SABIC Innovative Plastics Valox® 4631 PBT (Europe-Africa-Middle East)
VALOX 4631 is a 30% glass reinforced, flame retarded PBT injection moulding resin with good electrical properties and excellent mechanical properties.
Melt Flow 90 g/10 min

@Load 5.00 kg,
Temperature 266 °C
90 g/10 min

@Load 11.0 lb,
Temperature 511 °F
ASTM D1238
SABIC Innovative Plastics Valox® 4631 PBT (Europe-Africa-Middle East)